Ingá vs Ingá

Inga paraensis against Inga sp. Every number below names the publication it came from.

PropertyIngáIngá
Janka hardness3,064 lbfLPF/SFB Madeiras Brasileiras2,846 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC65.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-968.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture26,540 lb/in²LPF/SFB Madeiras Brasileiras22,915 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.60 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength12,090 lb/in²LPF/SFB Madeiras Brasileiras11,905 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.9%LPF/SFB Madeiras Brasileiras12.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.02LPF/SFB Madeiras Brasileiras2.34LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.