Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Inga-de-porco vs Albizzia

Albizia pedicellaris = Macrosamanea pedicellaris against Albizia spp.. Every number below names the publication it came from.

PropertyInga-de-porcoAlbizzia
Janka hardness955 lbfLPF/SFB Madeiras Brasileiras955 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC38.1 lb/ft³LPF/SFB Madeiras Brasileiras40.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture14,109 lb/in²LPF/SFB Madeiras Brasileiras8,855 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.69 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.06 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength7,253 lb/in²LPF/SFB Madeiras Brasileiras6,420 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)11.0%LPF/SFB Madeiras Brasileiras—
Tangential / radial ratio(lower is better)1.77LPF/SFB Madeiras Brasileiras—

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.