Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Ingá / ingá xixi vs Ingá

Inga alba against Inga sp. Every number below names the publication it came from.

PropertyIngá / ingá xixiIngá
Janka hardness1,418 lbfLPF/SFB Madeiras Brasileiras2,846 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC48.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-968.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture17,509 lb/in²LPF/SFB Madeiras Brasileiras22,915 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.93 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength8,733 lb/in²LPF/SFB Madeiras Brasileiras11,905 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.3%LPF/SFB Madeiras Brasileiras12.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.40LPF/SFB Madeiras Brasileiras2.34LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.