Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Janitá vs Conduru / pau-vermelho

Brosimum alicastrum against Brosimum rubescens. Every number below names the publication it came from.

PropertyJanitáConduru / pau-vermelho
Janka hardness2,059 lbfLPF/SFB Madeiras Brasileiras2,062 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-950.6 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture22,146 lb/in²LPF/SFB Madeiras Brasileiras20,609 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.32 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength12,502 lb/in²LPF/SFB Madeiras Brasileiras10,724 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.0%LPF/SFB Madeiras Brasileiras13.2%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.68LPF/SFB Madeiras Brasileiras1.47LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.