Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Jataipeba vs Ipe

Dialium guianense against Tabebuia spp., lapacho group. Every number below names the publication it came from.

PropertyJataipebaIpe
Janka hardness3,650 lbfLPF/SFB Madeiras Brasileiras3,680 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC63.7 lb/ft³LPF/SFB Madeiras Brasileiras70.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture24,614 lb/in²LPF/SFB Madeiras Brasileiras25,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,481 lb/in²LPF/SFB Madeiras Brasileiras13,010 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)14.5%LPF/SFB Madeiras Brasileiras13.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.75LPF/SFB Madeiras Brasileiras1.21USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.