Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Jelutong vs Okoume

Dyera costulata against Aucoumea klaineana. Every number below names the publication it came from.

PropertyJelutongOkoume
Janka hardness390 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b380 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC28.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)28.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture7,300 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b7,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.18 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength3,920 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3,970 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)7.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-411.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.39USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.49USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.