Kirikawa vs Ucuubarana

Iryanthera spp. against Iryanthera grandis. Every number below names the publication it came from.

PropertyKirikawaUcuubarana
Janka hardness930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,195 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC35.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)48.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture12,650 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)15,432 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.18 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.81 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,970 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)8,662 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)13.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.77Chudnoff 1984, Tropical Timbers of the World (AH-607)1.61LPF/SFB Madeiras Brasileiras

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.