Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Lama vs African ebony

Diospyros sandwicensis against Diospyros spp.. Every number below names the publication it came from.

PropertyLamaAfrican ebony
Janka hardness2,607 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a3,220 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-963.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture—21,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity——
Crushing strength—9,350 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—20.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)—1.17USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.