Leiteiro vs Burra-leiteira

Sapium glandulosum = Sapium aereum against Sapium marmieri. Every number below names the publication it came from.

PropertyLeiteiroBurra-leiteira
Janka hardness379 lbfLPF/SFB Madeiras Brasileiras324 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC32.5 lb/ft³LPF/SFB Madeiras Brasileiras30.0 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture10,156 lb/in²LPF/SFB Madeiras Brasileiras9,088 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.44 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,300 lb/in²LPF/SFB Madeiras Brasileiras4,722 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.1%LPF/SFB Madeiras Brasileiras10.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.86LPF/SFB Madeiras Brasileiras1.34LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons