Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Loblolly sweetwood vs East African Camphorwood

Ocotea leucoxylon against Ocotea usambarensis. Every number below names the publication it came from.

PropertyLoblolly sweetwoodEast African Camphorwood
Janka hardness915 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC37.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-937.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture—13,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity—1.44 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength—7,590 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)——

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.