Gambeya africana against Millettia spp.. Every number below names the publication it came from.

PropertyLonguiPanga Panga
Janka hardness1,658 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC48.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-955.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture—16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity—1.97 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength—9,950 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.40Chudnoff 1984, Tropical Timbers of the World (AH-607)1.87Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.