Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Louro-amarelo vs Kaneelhart

Licaria chrysophylla = Licaria rigida against Licaria spp.. Every number below names the publication it came from.

PropertyLouro-amareloKaneelhart
Janka hardness2,019 lbfLPF/SFB Madeiras Brasileiras2,900 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC57.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-962.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture24,010 lb/in²LPF/SFB Madeiras Brasileiras29,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras4.06 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,402 lb/in²LPF/SFB Madeiras Brasileiras17,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)13.5%LPF/SFB Madeiras Brasileiras12.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.72LPF/SFB Madeiras Brasileiras1.46USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.