PropertyLouro-mamorimLouro
Janka hardness1,135 lbfLPF/SFB Madeiras Brasileiras1,198 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC42.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-938.4 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture14,408 lb/in²LPF/SFB Madeiras Brasileiras15,651 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.46 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.81 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength8,150 lb/in²LPF/SFB Madeiras Brasileiras8,259 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)10.0%LPF/SFB Madeiras Brasileiras11.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.89LPF/SFB Madeiras Brasileiras2.17LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.