Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Mandioqueira vs Purpleheart

Ruizterania albiflora = Qualea albiflora against Peltogyne spp.. Every number below names the publication it came from.

PropertyMandioqueiraPurpleheart
Janka hardness1,351 lbfLPF/SFB Madeiras Brasileiras1,860 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC42.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture15,574 lb/in²LPF/SFB Madeiras Brasileiras19,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.86 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.27 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength8,306 lb/in²LPF/SFB Madeiras Brasileiras10,320 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)14.7%LPF/SFB Madeiras Brasileiras9.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.79LPF/SFB Madeiras Brasileiras1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.