Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Mandioqueira-escamosa vs Mandioqueira

Qualea dinizii against Qualea gracilior = Qualea cf lancifolia. Every number below names the publication it came from.

PropertyMandioqueira-escamosaMandioqueira
Janka hardness1,363 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,071 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC44.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-944.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture—15,603 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—1.82 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength—8,534 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—11.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—2.61LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.