PropertyMandioqueiraMandioqueira
Janka hardness1,071 lbfLPF/SFB Madeiras Brasileiras2,165 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC44.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture15,603 lb/in²LPF/SFB Madeiras Brasileiras19,145 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.82 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.26 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength8,534 lb/in²LPF/SFB Madeiras Brasileiras11,578 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)11.5%LPF/SFB Madeiras Brasileiras13.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.61LPF/SFB Madeiras Brasileiras1.95LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.