Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Matamatá vs Matamatá

Eschweilera coriacea against Eschweilera pedicellata = Eschweilera longipes. Every number below names the publication it came from.

PropertyMatamatáMatamatá
Janka hardness2,467 lbfLPF/SFB Madeiras Brasileiras2,410 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.2 lb/ft³LPF/SFB Madeiras Brasileiras61.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture19,002 lb/in²LPF/SFB Madeiras Brasileiras19,444 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.11 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,181 lb/in²LPF/SFB Madeiras Brasileiras9,673 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.0%LPF/SFB Madeiras Brasileiras14.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.71LPF/SFB Madeiras Brasileiras1.72LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.