Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Muiracatiara-rajada vs Goncalo alves

Astronium lecointei against Astronium graveolens. Every number below names the publication it came from.

PropertyMuiracatiara-rajadaGoncalo alves
Janka hardness2,051 lbfLPF/SFB Madeiras Brasileiras2,160 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC61.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-967.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,453 lb/in²LPF/SFB Madeiras Brasileiras16,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.03 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.23 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,076 lb/in²LPF/SFB Madeiras Brasileiras10,320 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)11.0%LPF/SFB Madeiras Brasileiras10.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.76LPF/SFB Madeiras Brasileiras1.90USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.