Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Muirapixuna vs Cumaru

Chamaecrista scleroxylon = Cassia scleroxylon against Dipteryx odorata. Every number below names the publication it came from.

PropertyMuirapixunaCumaru
Janka hardness3,435 lbfLPF/SFB Madeiras Brasileiras3,415 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC84.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-966.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture26,227 lb/in²LPF/SFB Madeiras Brasileiras24,371 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,967 lb/in²LPF/SFB Madeiras Brasileiras14,742 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)11.5%LPF/SFB Madeiras Brasileiras13.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.28LPF/SFB Madeiras Brasileiras1.56LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.