Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Muiratinga vs Purpleheart

Maquira sclerophylla against Peltogyne spp.. Every number below names the publication it came from.

PropertyMuiratingaPurpleheart
Janka hardness1,389 lbfLPF/SFB Madeiras Brasileiras1,860 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC43.8 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture16,059 lb/in²LPF/SFB Madeiras Brasileiras19,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.64 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.27 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength8,791 lb/in²LPF/SFB Madeiras Brasileiras10,320 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)13.7%LPF/SFB Madeiras Brasileiras9.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.24LPF/SFB Madeiras Brasileiras1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.