Mururé vs Garrote

Brosimum acutifolium subsp interjectum against Brosimum sp. Every number below names the publication it came from.

PropertyMururéGarrote
Janka hardness1,120 lbfLPF/SFB Madeiras Brasileiras1,074 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC42.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-936.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture14,508 lb/in²LPF/SFB Madeiras Brasileiras13,526 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.69 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.69 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength7,922 lb/in²LPF/SFB Madeiras Brasileiras7,467 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.6%LPF/SFB Madeiras Brasileiras0.7%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.63LPF/SFB Madeiras Brasileiras1.40LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.