PropertyOhiaAndaman Padauk
Janka hardness2,090 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC57.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)48.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture18,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Modulus of elasticity2.37 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength8,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Volumetric shrinkage(lower is better)—6.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.33Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.