Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Old-growth redwood vs Young-growth redwood

Sequoia sempervirens against Sequoia sempervirens. Every number below names the publication it came from.

PropertyOld-growth redwoodYoung-growth redwood
Janka hardness480 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b420 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC28.0 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b24.5 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture10,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b7,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.34 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.10 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength6,150 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b5,220 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)6.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-37.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)1.69USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-32.23USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • manual map (regional variant)public domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.