PropertyOpepePanga Panga
Janka hardness1,630 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC47.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture17,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.94 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.97 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b9,950 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)12.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—
Tangential / radial ratio(lower is better)1.87USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.87Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.