Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Osage orange vs European yew

Maclura pomifera against Taxus baccata. Every number below names the publication it came from.

PropertyOsage orangeEuropean yew
Janka hardness2,607 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,009 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a
Density at 12% MC60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-945.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture——
Modulus of elasticity——
Crushing strength——
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)——

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.