PropertyOvercup oakBlack oak
Janka hardness1,190 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1,210 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC44.1 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b42.6 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture12,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b13,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.42 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.64 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength6,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b6,520 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)16.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-315.1%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)2.40USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-32.52USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.