Parana-pine vs Radiata pine

Araucaria augustifolia against Pinus radiata. Every number below names the publication it came from.

PropertyParana-pineRadiata pine
Janka hardness780 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b750 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC34.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-931.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture13,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b11,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.61 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.48 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength7,660 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b6,080 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)11.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—
Tangential / radial ratio(lower is better)1.98USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.