Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Pau-de-jangada vs Duru

Apeiba echinata against Apeiba spp.. Every number below names the publication it came from.

PropertyPau-de-jangadaDuru
Janka hardness558 lbfLPF/SFB Madeiras Brasileiras250 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC26.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-914.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture7,667 lb/in²LPF/SFB Madeiras Brasileiras4,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity0.97 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras—
Crushing strength4,608 lb/in²LPF/SFB Madeiras Brasileiras670 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)9.3%LPF/SFB Madeiras Brasileiras7.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)2.83LPF/SFB Madeiras Brasileiras3.00Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.