Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Pau marfim vs Canalete

Balfourodendron riedelianum against Cordia spp. (hard-wooded, dark-colored Gerascanthus group). Every number below names the publication it came from.

PropertyPau marfimCanalete
Janka hardness2,367 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC57.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture18,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b—
Modulus of elasticity——
Crushing strength8,190 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b—
Volumetric shrinkage(lower is better)13.4%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-411.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.85Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.