Pau-santo vs Cumaru

Zollernia paraensis against Dipteryx odorata. Every number below names the publication it came from.

PropertyPau-santoCumaru
Janka hardness3,261 lbfLPF/SFB Madeiras Brasileiras3,415 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC78.7 lb/ft³LPF/SFB Madeiras Brasileiras66.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture27,238 lb/in²LPF/SFB Madeiras Brasileiras24,371 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.59 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,854 lb/in²LPF/SFB Madeiras Brasileiras14,742 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.8%LPF/SFB Madeiras Brasileiras13.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.92LPF/SFB Madeiras Brasileiras1.56LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.