PropertyPequiáPequiarana
Janka hardness1,133 lbfLPF/SFB Madeiras Brasileiras1,642 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC48.7 lb/ft³LPF/SFB Madeiras Brasileiras48.7 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture14,479 lb/in²LPF/SFB Madeiras Brasileiras11,464 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.62 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.01 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,741 lb/in²LPF/SFB Madeiras Brasileiras8,505 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.6%LPF/SFB Madeiras Brasileiras11.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.98LPF/SFB Madeiras Brasileiras2.20LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain