Ponderosa pine vs Lodgepole pine

Pinus ponderosa against Pinus contorta. Every number below names the publication it came from.

PropertyPonderosa pineLodgepole pine
Janka hardness460 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b480 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC28.0 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b28.7 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture9,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b9,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.29 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.34 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength5,320 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b5,370 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)9.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-311.1%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.56USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.