PropertyPride-of-BarbadosAndaman Padauk
Janka hardness1,598 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC48.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-948.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture——
Modulus of elasticity——
Crushing strength——
Volumetric shrinkage(lower is better)—6.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.33Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain