Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Purpleheart vs Angico

Peltogyne spp. against Peltogyne cf subsessilis. Every number below names the publication it came from.

PropertyPurpleheartAngico
Janka hardness1,860 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,941 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)60.6 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture19,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b22,971 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.27 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.28 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,320 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b17,168 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)9.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-413.4%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.75LPF/SFB Madeiras Brasileiras

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.