Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Quaruba vs Quaruba

Vochysia obidensis against Vochysia maxima. Every number below names the publication it came from.

PropertyQuarubaQuaruba
Janka hardness1,179 lbfLPF/SFB Madeiras Brasileiras976 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC38.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-936.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture14,594 lb/in²LPF/SFB Madeiras Brasileiras12,538 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.81 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength7,681 lb/in²LPF/SFB Madeiras Brasileiras6,692 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.7%LPF/SFB Madeiras Brasileiras12.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)3.13LPF/SFB Madeiras Brasileiras2.20LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.