PropertyRed alderTrue mahogany
Janka hardness590 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b800 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC28.7 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b41.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture9,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b11,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.38 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.50 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength5,820 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b6,780 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)12.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-37.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.66USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.37USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.