Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Red maple vs Bigleaf maple

Acer rubrum against Acer macrophyllum. Every number below names the publication it came from.

PropertyRed mapleBigleaf maple
Janka hardness950 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b850 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC37.8 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b33.6 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture13,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b10,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.64 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.45 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength6,540 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b5,950 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)12.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-311.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)2.05USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.92USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.