PropertySandeJanitá / garrote
Janka hardness900 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b946 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC37.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-936.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture14,300 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b11,008 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.39 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.65 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength8,220 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b6,685 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-412.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.74USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.59LPF/SFB Madeiras Brasileiras

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0