Sapucaia / sapucaia-vermelha vs Sapucaia

Lecythis pisonis subsp. usitata against Lecythis spp.. Every number below names the publication it came from.

PropertySapucaia / sapucaia-vermelhaSapucaia
Janka hardness2,831 lbfLPF/SFB Madeiras Brasileiras3,100 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture21,747 lb/in²LPF/SFB Madeiras Brasileiras27,540 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.38 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,185 lb/in²LPF/SFB Madeiras Brasileiras13,280 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)13.9%LPF/SFB Madeiras Brasileiras13.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.43LPF/SFB Madeiras Brasileiras1.27Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.