Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Satinleaf vs Goiabão

Chrysophyllum oliviforme against Chrysophyllum lucentifolium = Pouteria pachycarpa. Every number below names the publication it came from.

PropertySatinleafGoiabão
Janka hardness2,607 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a2,646 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.1 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture—22,999 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—2.41 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength—11,357 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—16.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—1.81LPF/SFB Madeiras Brasileiras

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.