Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Sea vs Burada

Parinari insularum against Parinari spp.. Every number below names the publication it came from.

PropertySeaBurada
Janka hardness1,852 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,830 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC51.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-952.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture—20,120 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity—2.61 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength—10,260 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—14.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.69Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.