Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Sepetir vs Merbau

Pseudosindora palustris against Intsia spp.. Every number below names the publication it came from.

PropertySepetirMerbau
Janka hardness1,410 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1,500 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC42.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)50.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture17,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b16,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.97 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.23 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength8,880 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b8,440 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)10.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-47.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.89USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.70USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.