PropertyShagbark hickoryPecan hickory
Janka hardness1,880 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1,820 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC50.3 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b46.1 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture20,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b13,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity2.16 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.73 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength9,210 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b7,850 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)16.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-313.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)1.50USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.82USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • manual map (regional variant)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.