Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Shorea vs White meranti

Shorea spp., bullau group against Shorea spp.. Every number below names the publication it came from.

PropertyShoreaWhite meranti
Janka hardness1,780 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1,140 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC53.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-942.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture18,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b12,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.61 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.49 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength10,180 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b6,350 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)——

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.