Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Spanish-cedar vs Toon

Cedrela spp. against Cedrela spp. (mainly C toona). Every number below names the publication it came from.

PropertySpanish-cedarToon
Janka hardness600 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b550 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC35.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)31.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture11,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b10,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.44 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.30 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength6,210 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3,480 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)10.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-410.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.50USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.66Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.