Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Tamboril vs Guanacaste

Enterolobium maximum against Enterolobium cyclocarpum. Every number below names the publication it came from.

PropertyTamborilGuanacaste
Janka hardness691 lbfLPF/SFB Madeiras Brasileiras520 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC29.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-926.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture9,487 lb/in²LPF/SFB Madeiras Brasileiras8,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength5,817 lb/in²LPF/SFB Madeiras Brasileiras4,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)6.7%LPF/SFB Madeiras Brasileiras7.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.88LPF/SFB Madeiras Brasileiras2.60Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.