PropertyTanimbucaIndian Laurel
Janka hardness2,235 lbfLPF/SFB Madeiras Brasileiras2,220 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-954.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture21,178 lb/in²LPF/SFB Madeiras Brasileiras15,380 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.03 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.91 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength11,307 lb/in²LPF/SFB Madeiras Brasileiras8,275 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)12.8%LPF/SFB Madeiras Brasileiras13.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.50LPF/SFB Madeiras Brasileiras1.54Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.