Tasmanian-Myrtle vs Rauli

Nothofagus spp. against Nothofagus spp.. Every number below names the publication it came from.

PropertyTasmanian-MyrtleRauli
Janka hardness1,325 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)990 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC39.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)37.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture15,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.97 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.49 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength8,170 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)6,650 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)——

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.