Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Taxi-branco vs Pau-ponga

Tachigali cavipes against Tachigali sp.. Every number below names the publication it came from.

PropertyTaxi-brancoPau-ponga
Janka hardness818 lbfLPF/SFB Madeiras Brasileiras1,019 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC34.3 lb/ft³LPF/SFB Madeiras Brasileiras36.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture11,934 lb/in²LPF/SFB Madeiras Brasileiras13,840 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.48 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.54 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,443 lb/in²LPF/SFB Madeiras Brasileiras6,812 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)9.7%LPF/SFB Madeiras Brasileiras11.9%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.38LPF/SFB Madeiras Brasileiras1.72LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.