Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Taxi-pitomba vs Taxi

Tachigali poeppigiana = Sclerolobium poeppigianum against Tachigali glauca = Tachigali myrmecophila. Every number below names the publication it came from.

PropertyTaxi-pitombaTaxi
Janka hardness1,479 lbfLPF/SFB Madeiras Brasileiras1,505 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC50.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-943.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture18,675 lb/in²LPF/SFB Madeiras Brasileiras17,082 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.91 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.73 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,815 lb/in²LPF/SFB Madeiras Brasileiras8,278 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.6%LPF/SFB Madeiras Brasileiras11.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.93LPF/SFB Madeiras Brasileiras1.78LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.